by IgorPartola · 10mo ago · 0 comments
Another note: PLA has gotten significantly better in the past few years. PLA+ is legitimately better while being as easy to print and the Polymaker HT-PLA and HT-PLA-GF are even better as you can meaningfully anneal them after printing to make them strong and temperature resistant enough for some very functional prints.
In the garage, I have one that I can slap down anywhere, with a couple boxes that I can load for the screws, nails, washers, nuts, and bolts, etc... used in my current project.
Having the grid makes the boxes sit firmly in place.
And in that sense it means that almost every design made by someone else you find will fit your machine. I rarely if ever find something on Printables or Makerworld that requires a larger machine than the A1.
Then you’ve got the A1 mini being ao popular that many times people will make variants just for the small plate on that machine.
One thing I've started playing with now are gridfinity cases so I can pick a bunch of part boxes out of my drawers, put them in the case and take them to the garage without risk of everything falling out. Then, when I'm done, they go back in the drawer.
For functional parts I would not use anything else until there is a really good reason (such as high temperature stability or more strength for a given weight or cross section). I've gone through multiple tons of the stuff now (3500 Kg in total or so) on 85 printers (Bambu's (43), Creality (22) K1s and Prusas (20)), consistency between batches is very good though from brand to brand there can be some notable differences.
If you have stringing and globbing problems with PETG my first guess would be that the filament profile that you are using is subtly off for that particular brand of PETG and/or that the filament wasn't dry.
PETG is just oozier and stickier by default, so stringiness is almost guaranteed to happen, bridging at a greater risk of failure, etc. It is tougher, so unless you have a printer that can use multiple filaments on the same print, removing supports is more difficult.
Can you reduce these factors by tuning your 3D printer - yes, a bit. But that's not "utterly problem free".
PLA is the plug and play of the 3D printing world right now.
I personally run all PETG because it is ultimately better material post-print, and once you understand how to print with it, it’s not really much harder to deal with.
The day I discovered that I should just run my dryer with the PETG inside while printing was revolutionary. Of course, that requires you own a dryer that allows the filament to print while it’s inside.
I am getting reasonably consistent prints but they aren't perfect.
The long version of my tips for using PETG are:
- A Bambu Lab printer doesn't hurt since it's so nicely calibrated and idiot-proof
- Clean the build plate with dish soap and dry fully. I haven't found any need for glue stick on a textured plate.
- Using a filament that has a profile available from the manufacturer for Bambu lab printers
- Printing with the filament in the dryer with the dryer running during printing
I can print PLA at 100mm/s with .25mm layers...but PETG I don't go much over 65mm/s give the same line width/layer height.
Since getting things dialed in I switched to primarily printing PETG. Although, I have no issue printing PLA, PETG or ABS when needed.
Better ratio of weight to strength, far more durable parts for most jobs, and acetone smoothening opens up all sorts of doors to incredibly high quality prints without all the labor of sanding.