by fsilva · 17y ago · 0 comments
about an alternative to ferric cloride, acid cupric cloride. It is easier to buy, since all you are doing is mixing 2 parts oxygenated water with 1 part muriatic acid/HCl (@33%), which can be obtained at any hardware store. It shares the same problem with Ferric Cloride: after etching, the resulting solution is hazardous and should be disposed accordingly (€€/$$).
I've done this at home just like the original article but with this other solution and after 3-4 tries got pretty good results. Good enough for some basic SMD circuits.